Gold filled
Gold filled describes jewelry with a base-metal core, usually brass, covered by a thick layer of karat gold that is bonded on mechanically rather than electroplated. Under the FTC's jewelry guides, a piece can be called gold filled when that layer is at least 10K gold and makes up at least 1/20 of the metal's weight.
From JewelryRepair.com: over 50,000 repairs since 1989 · 4.9 from 187 Google reviews (as of )
What gold filled means
Gold filled is a construction, not an alloy: a distinct layer of karat gold over a base-metal core. Cookson Gold, a jewelry metals supplier, describes the core as usually brass and the gold as bonded to it with heat and pressure, a permanent bond that won't flake or peel. The FTC's jewelry guides are the US standard for how jewelry is described. Under them, "gold filled" fits when a layer of gold alloy of at least 10 karat is joined to all significant surfaces by soldering, brazing, welding or other mechanical means and makes up at least 1/20 of the weight of all the metal in the piece, which is 5%. From 1/40 of the weight, the guides allow "gold plate", "gold overlay" or "rolled gold plate" with the karat, and overlay or rolled gold plate with the fraction stated too, as in their example "1/40 12 Kt. R.G.P."; "gold filled" takes at least 1/20.
The arithmetic shows how far it is from solid gold. A 1/20 14K gold-filled piece is 5% gold alloy by weight, and 14K alloy is 58.3% gold, so the piece is about 2.9% pure gold (0.05 × 0.583). A 10-gram 1/20 14K gold-filled chain carries about 0.29 grams of pure gold; a solid 14K chain of the same weight carries about 5.8 grams.
How to read the marks
- GF, G.F. or Gold Filled with a karat, often with a fraction: 1/20 14K GF, 12K G.F., usually on the clasp, a tag or inside a ring shank.
- RGP or Rolled Gold Plate: the same bonded construction from 1/40 of the weight, marked with the fraction, as in 1/40 12K RGP.
- GP or Gold Plated: can mean electroplate, or, under the FTC guides, a mechanically bonded layer of at least 1/40 of the weight, so the mark alone doesn't say which.
- GEP or Gold Electroplate: electroplated, a much thinner layer; HGE is heavy gold electroplate.
- 14K, 585, 18K or 750 on its own: solid karat gold, if the stamp is honest; see what 585, 750 and 925 stamps mean.
Two cautions. When gold-filled products are assayed, the guides leave out small working parts such as springs, catches and joints, so expect those to be base metal even on honest gold filled. And stamps can be wrong: our metal testing checks hallmarks under magnification for the soft edges and misplaced positions of counterfeit stamps, then tests the metal itself, because heavy plating over base metal is the most common surprise in inherited jewelry.
Gold filled vs gold plated
Both put real gold over a cheaper metal; the difference is how much gold, and how it is attached. Gold filled is bonded mechanically and measured by weight: at least 1/20 of the metal. Gold electroplate is deposited by electric current and measured by thickness: in the guides' example, 0.175 microns of fine gold, about 7 millionths of an inch, for "gold electroplate" and 2.5 microns for "heavy gold electroplate". Those are thresholds for the names, not limits on how thin plating can be. By Cookson Gold's figures, gold usually makes up under 0.05% of a plated item's total weight; in gold filled it is at least 5% gold alloy, about 2.9% pure gold at 14K. With far more gold to wear through, gold filled generally wears longer. For the plated categories, see gold plating and vermeil.
How gold filled wears, and how repairs work here
Gold filled wears like a very thick plating, slowly, from the points that rub; our answer on whether gold filled tarnishes covers where it shows first and how to look after it. The bigger risks come at the bench. Any cut exposes the core at the cut edges, filing and polishing a solder joint can go through the gold layer at the repair, and heavy polishing anywhere takes gold off the surface.
Gold filled isn't listed as a metal on our ring and chain repair pages, so we recommend asking for a free, itemized quote through the contact page first: a jeweler answers within 1 business day, and you see the price before anything ships. The $19 Mail-In Evaluation is the other route, and the $19 comes off the work you approve.
Signs your gold-filled piece needs attention
- A brassy patch at the clasp, on the back of a ring or along an edge: the core is showing. Gold Plating can put the color back.
- A green mark on your skin from one spot: usually copper in the brass core reaching the skin where the gold has worn through; see why a ring turns a finger green.
- A broken link or a clasp that won't hold: ask for a free quote first, as above.
- You're not sure it's gold filled at all: Metal Testing & Verification, $15 per item.
What it costs here
Re-plating a worn gold-filled ring or pendant on a brass base is $173 with flash plating ($60 + $113), and a thicker 1–2 micron layer adds $250. New plating brings back the color; the bonded gold layer itself can't be rebuilt. Keep the metal value in proportion too: by the arithmetic above, a 10-gram 1/20 14K chain holds about 0.29 grams of pure gold, so the case for repairing it is the piece itself, not the gold in it.
Every metal test at our New York studio ends in a documented result. Sky Jewelry, which runs JewelryRepair.com, has been a family jeweler on Lenox Avenue since 1989.
Prices at a glance
| Service | Price | What's included |
|---|---|---|
| Metal Testing & Verification | $15 | Hallmarks and stamps examined under magnification, then the metal tested directly and cross-checked when a first result is ambiguous. You get a documented result. |
| Mail-In Evaluation | $19 | For soldering, sizing or clasp work on gold filled: a jeweler examines the piece and sends an itemized quote with photos. The $19 is credited in full toward the work you approve. |
| Gold Plating | $173 ring, brass base, flash | Fresh electroplated gold once the gold-filled layer has worn through, after a full polish, cleaning and activation. A 1–2 micron layer adds $250. The jeweler confirms the base metal first. |
Prices come from the live repair pages. Shipping is $30 round trip per order.
Related questions
Questions
Is gold filled real gold?
How can I tell if my jewelry is gold filled?
Can gold filled jewelry be repaired?
Can worn gold filled be re-plated?
Is gold filled better than gold plated?