Metals & plating

Sterling silver

Hands polishing a ring against a spinning polishing wheel

Sterling silver is an alloy of at least 92.5% pure silver, with the rest usually copper, which is why sterling jewelry is stamped 925. Pure silver bends and scuffs too easily for daily wear; the copper adds strength but also speeds up tarnish. US law sets 925 parts per thousand as the sterling standard, with a small assay tolerance.

From JewelryRepair.com: over 50,000 repairs since 1989 · 4.9 from 187 Google reviews (as of )

What sterling silver is

Sterling is an alloy: 925 parts pure silver per 1,000, with the other 75 parts usually copper. Pure silver bends and scuffs too easily for a ring shank or a clasp spring, so a little copper is mixed in for strength.

The standard is set in US rules. The Federal Trade Commission's jewelry guides say a product shouldn't be described as "Sterling Silver," "Sterling," "Ster." or "solid silver" unless it is at least 925/1,000ths pure silver, and the National Stamping Act bars silver-plated articles from being stamped "sterling." The Act also allows a small assay tolerance: four parts per thousand, or ten where the tested part contains solder, as the FTC guide notes. The marks to look for are 925, Sterling or Ster., usually inside a ring band or on a small tag near a clasp.

Why sterling tarnishes

Tarnish is a chemical reaction, not dirt. Silver reacts with sulfur gases in the air, mainly hydrogen sulfide, to form silver sulfide; in sterling, the copper forms copper sulfide as well. Because copper is more reactive than silver, sterling tarnishes faster than pure silver. The color shows how thick the layer has grown: it shifts from yellow through red-brown to blue, and a heavy layer looks black. Humidity speeds it up, and so do sulfur sources such as rubber bands, wool felt and eggs.

To slow it down, the Canadian Conservation Institute recommends keeping silver dry (below 50% relative humidity), sealed in polyethylene bags with acid-free tissue, and adding silica gel, activated charcoal or an anti-tarnish cloth. Every polish removes a little silver, so polish when it's needed, not on a schedule. For light tarnish, the institute finds a silver polishing cloth most useful, warns against general multi-purpose metal polishes, and says chemical dips should never be used on pieces with sealed hollow parts. Step by step: how to clean tarnished sterling silver jewelry.

Why it matters for repairs

  • Firescale: heating sterling in air oxidizes the copper in the alloy. Surface scale cleans off, but oxygen can also work below the surface and leave a reddish-purple stain, called firescale or firestain, that often shows up during polishing. Silversmiths limit it with protective coatings and careful heating, and removing it means taking off metal or covering it with plating.
  • Thin spots: years of wear thin a silver band at the bottom and tire out clasp springs and jump rings. A cracked band can be soldered, and a band worn thin can be re-shanked with new metal.
  • Plating hides the metal: some sterling is rhodium-plated, and vermeil is sterling coated with gold of at least 10 karat. Polishing or soldering through that layer leaves a spot that has to be re-plated to match.
  • Silver is the base price: on most repair pages here, sterling is the metal with no surcharge, so silver work usually costs the least.

How to tell if it's sterling

  • Look for the mark: 925, Sterling or Ster.
  • Look at worn edges: on a plated piece, a different-colored metal often shows through at edges and high points. Sterling is silver all the way through.
  • Tarnish proves nothing: silver plate tarnishes too, because its surface is silver.
  • Watch the names: "nickel silver" and "German silver" contain no silver at all; they're copper, nickel and zinc. EPNS means electroplated nickel silver, a silver-plated version of that alloy.
  • Test it: stamps can be wrong, and unmarked pieces tell you nothing. Metal Testing & Verification is $15 per item: hallmarks checked, metal tested and documented.

Sterling silver vs silver plated

Silver-plated jewelry is a base metal, such as copper or nickel silver, with a thin coat of silver on its surface. Under the FTC guides, a piece can only be called silver-plated if all its significant surfaces carry a reasonably durable silver coating, and it can't be stamped sterling. The difference shows over time and at the bench. Sterling can be polished, soldered, resized and refinished again and again because it's the same metal throughout. Plating wears through, and the Canadian Conservation Institute warns that any method of tarnish removal can be very damaging to silver plate. Plated pieces take a different route here: Jewelry Polishing has no plated option, so a silver-plated piece that needs polishing goes to a free quote. For solder work, Chain Soldering, Ring Resizing and Earring Post Repair list a "Gold-plated / fashion" metal choice; if you aren't sure what your piece is made of, start with a free quote.

What it costs here

Sterling is the no-surcharge metal on most JewelryRepair.com repair pages, so the starting price is the silver price:

Every repair price includes a clean and polish, and shipping is $30 round trip per order by UPS. The 1-year workmanship guarantee covers a solder joint that reopens, and Sky Jewelry's New York studio has done over 50,000 repairs since 1989.

Prices at a glance

Service Price What's included
Jewelry Polishing from $30 Machine and hand polishing to a mirror, satin or brushed finish. In silver: $30 for a ring or earrings, $50 for a bracelet, $60 for a pendant, $105 for a necklace.
Jewelry Spa from $44 A standalone ultrasonic, steam and hand-polish clean with a written inspection report; $56 for a silver bracelet or necklace.
Rhodium Plating from $69 Polish, clean and a fresh layer of rhodium, a platinum-family metal, for a bright white finish. Oxidation +$28 or black rhodium +$24 for a darker look.
Chain Soldering from $30 One break in a sterling chain soldered and polished flush, or laser-welded on hollow chains. Two breaks +$17; hollow +$20.
Ring Resizing from $45 In silver: $45 to size down, $50 to size up one size, +$35 for each extra full size up. Sized with matching stock, soldered and polished.
Shank Repair from $45 A cracked or cut band repaired. A worn-thin silver band can get a new half band (+$75) or full band (+$125); in other metals those are +$250 and +$375.
Metal Testing & Verification $15 Hallmarks checked and the metal tested and documented, for an unmarked piece or a 925 stamp you doubt.

Prices come from the live repair pages. Shipping is $30 round trip per order.

Questions

What does 925 mean on jewelry?
It means the metal is sterling silver: at least 925 parts pure silver per 1,000, or 92.5%, with the rest usually copper. Under the US Federal Trade Commission's jewelry guides, only silver at that standard may be called Sterling Silver, Sterling or Ster. If a 925 stamp looks doubtful, Metal Testing & Verification at JewelryRepair.com checks the hallmark and tests the metal for $15 per item.
Why does sterling silver turn black?
Because it tarnishes. Silver reacts with sulfur gases in the air, mainly hydrogen sulfide, to form silver sulfide, and the copper in sterling forms copper sulfide too. Thin layers look yellow or brown and thick layers look black. Humidity and sulfur sources such as rubber bands and wool speed it up. Jewelry Polishing at JewelryRepair.com restores the finish from $30 for a silver ring.
Is sterling silver real silver?
Yes. Sterling is at least 92.5% pure silver, with a small amount of another metal, usually copper, added because pure silver alone bends too easily for everyday jewelry. Silver-plated pieces are different: a base metal with a thin silver coat that can wear through. "Nickel silver" and "German silver" contain no silver at all. Metal Testing & Verification at JewelryRepair.com confirms what you have for $15 per item.
Can sterling silver be resized or soldered?
Yes, and it's usually the least expensive metal to repair, because silver carries no metal surcharge on most services. At JewelryRepair.com, Ring Resizing is $45 to size a sterling ring down and $50 to size it up one size, and Chain Soldering is $30 for one break. Every repair price includes a clean and polish, and the piece is photographed before it ships back.
Can you rhodium plate sterling silver?
Yes. Rhodium Plating at JewelryRepair.com is $69 for a sterling silver ring: the piece is polished, cleaned and given a fresh layer of rhodium, a platinum-family metal, for a bright white finish. For a darker look, oxidation adds $28 and black rhodium $24. Plating is a surface layer, so it wears with time on high-contact spots and can be redone.